Sherafina 2000 160g cardboard 38pcs.
SHERAFINA 2000
Refractory mass for crowns and bridges:
- perfect quality
- for injection porcelain
- for alloys of precious and non-precious metals
- easy expansion control
- for quick and slow heating
- very fine-grained and compact consistency
- smooth surface of castings
- very high accuracy of castings
Package:
- Carton 38x160 g
Sherafina Rapid 160g carton 38pcs.
SHERAFINA-RAPID
Investment material for crowns and bridges:
- for alloys of precious and non-precious metals
- easy expansion control
- for quick and slow heating
- very fine-grained and compact consistency
- smooth surface of castings
- very high accuracy of castings
Package:
- Carton 38x160 g
Sheracast 2000 400g cardboard 25pcs.
SHERACAST 2000
Investment material for frameworks:
- perfect quality
- for quick and slow heating
- for silicone mirroring
- high accuracy of castings
- smooth surface of castings
- the oxides bind to the mass as the casting is released
Package:
- Cardboard 25x400g
IPS PressVEST Premium Powder 5kg (50x100g)
Product description:
- IPS PressVest Premium is a universal phosphate investment (type 1, class 1 and 2) that can be used with ceramic stamping materials in Ivoclar Vivadent furnaces.
- It can be used both in the speed heating procedure and in the conventional procedure.
"Speed" heating procedure:
- The ring is placed in a furnace heated to its final temperature and then transferred to a pressing furnace after a certain time.
Conventional annealing procedure:
- The ring is placed in a non-heated oven (room temperature) and heated to its final temperature as recommended. After the specified time, the ring is transferred to a pressing furnace.
Indications:
IPS Press VEST Premium can be used with the following ceramic stamping materials in Ivoclar Vivadent furnaces
IPS e.max Press
- IPS e.max ZirPress
- IPS InLine PoM (Press- on Metal)
Storage:
- Store at 12-28 ° C
- Store the powder in a dry place
- Do not store the liquid at temperatures below +5 ° C (because of its sensitivity to low temperatures!). If the fluid freezes, it becomes unusable due to crystallization.
Temperature at which the material can be used:
- Ambient temperature 18 ° C - max. 23 ° C.
- Temperature significantly deviating from this range may significantly affect the setting process.
- Lower ambient temperature slows down the chemical process.
- Higher ambient temperature accelerates the chemical process (from 23 - 28 ° C, the liquid with water can be cooled down to 12 ° C.
Mixing ratio:
By diluting the liquid, it is possible to control the expansion of the investment material, which influences the fit of the pressed restoration. The concentration of the liquid is expressed in%. Important: The ratio of the amount of mixed liquid (liquid to investment material + distilled water) depends on the amount of powder and must be strictly adhered to.
100 g of powder: 26 ml of liquid (investment liquid + distilled water)
- 200 g of powder: 52 ml of liquid (investment fluid + distilled water)
- 300 g of powder: 78 ml of liquid (investment liquid + distilled water)
The following information regarding fluid concentrations is a guide only and may be adjusted based on application and mixing conditions. Do not dilute the fluid to a level below 50%!
Packaging:
- 50 x 100g.